C94300 High Leaded Tin Bronze (Soft Bronze)
Typical Uses for C94300 High Leaded Tin Bronze (Soft Bronze):
INDUSTRIAL: High Speed, Light to Medium Pressure Bushings, Railroad Applications, Soft Bushings, High Speed Bearings for Light Loads, Soft Metal Applications
Product Type |
Temper Type |
Continuous |
ASTM B505, SAE J461, J462 |
Ingot |
ASTM B30 |
Sand |
ASTM B584, B763, SAE J461, J462 |
Temper |
Sect. Size |
Cold Work |
Type Min |
Temp |
Tensile Strength |
YS 0.05% UL |
YS 0.02% Offset |
YS 0.005% Offset |
Elong. |
RH B |
RH C |
RH F |
RH 30T |
VH 500 |
BH 500 |
BH 3000 |
Shear Strgth |
Fatigue Strgth |
Izod Impact Strgth |
- |
in. |
% |
- |
F |
ksi |
ksi |
ksi |
ksi |
% |
B |
C |
F |
30T |
500 |
500 |
3000 |
ksi |
ksi |
ft-lb |
- |
mm. |
- |
- |
C |
MPa |
MPa |
MPa |
MPa |
- |
- |
- |
- |
- |
- |
- |
- |
MPa |
MPa |
J |
As Continous Cast |
TF00 |
|
|
|
68 |
75 |
50 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
|
TF00 |
|
0 |
SMIN |
20 |
517 |
345 |
- |
- |
5 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
0 |
M07 |
|
|
|
68 |
45 |
20 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
|
M07 |
|
0 |
SMIN |
20 |
310 |
138 |
- |
- |
25 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
0 |
As Sand Cast |
M01 |
|
|
|
68 |
75 |
50 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
|
M01 |
|
0 |
SMIN |
20 |
517 |
345 |
- |
- |
5 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
0 |
M01 |
|
|
|
68 |
45 |
20 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
|
M01 |
|
0 |
SMIN |
20 |
310 |
138 |
- |
- |
25 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
0 |
M01 |
|
|
|
68 |
50 |
23 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
38 |
14 |
85 |
M01 |
|
0 |
TYP |
20 |
345 |
159 |
- |
- |
35 |
- |
- |
- |
- |
- |
85 |
- |
262 |
97 |
115 |
TF00 |
|
|
|
68 |
85 |
60 |
- |
- |
- |
- |
- |
- |
- |
- |
- |
190 |
65 |
14 |
110 |
TF00 |
|
0 |
TYP |
20 |
586 |
414 |
- |
- |
10 |
- |
- |
- |
- |
- |
- |
190 |
448 |
97 |
149 |
Product Property |
US Customary |
Metric |
Coefficient of Thermal Expansion |
10.9 . 10-6 per oF (68-392 F) |
19.6 . 10-6 per oC (20-300 C) |
Density |
0.32 lb/in3 at 68 F |
8.86 gm/cm3 @ 20 C |
Electrical Conductivity |
12 %IACS @ 68 F |
0.066 MegaSiemens/cm @ 20 C |
Melting Point - Liquidus |
1880 F |
1027 C |
Melting Point - Solidus |
1660 F |
904 C |
Modulas of Elasticity in Tension |
10500 ksi |
103400 MPa |
Specific Gravity |
8.86 |
8.86 |
Specific Heat Capacity |
0.09 Btu/lb/oF at 68 F |
377.1 J/kg . oK at 293 K |
Thermal Conductivity |
31.2 Btu . ft/(hr . ft2 . oF)at 68F |
54.0 W/m . oK at 20 C |
Joining Technique |
Suitability |
Brazing |
Poor |
Coated Metal Arc Welding |
Not Recommended |
Gas Shielded Arc Welding |
Not Recommended |
Machinability Rating |
80 |
Oxyacetylene Welding |
Not Recommended |
Soldering |
Good |
End Product |
Specification |
Continuous |
ASTM B505, SAE J461, J462 |
Ingot |
ASTM B30 |
Sand |
ASTM B584, B763, SAE J461, J462 |